Item Description Testing Method
D10 (μm) ≤ 5.0 Laser Particle Size Analyzer
D50 (μm) 10.0-14.0
D90 (μm) ≥25.0
Appearance Dark brown powder, atmospheric stability
Elements Proportions Ni:Co:Mn = 5:2:3
Ni+Co+Mn (%) ≥58 Volumetry
Li (%) 7.00-8.00 Atomic Absorption Spectroscopy
Inductively Coupled Plasma
Fe (%) ≤0.01
Na (%) ≤0.03
Cu (%) ≤0.005
H2O (%) ≤0.05 Coulometric KF Titrator
PH ≤ 11.50 PH Tester
H2O (%) ≤ 0.1 Moisture Analyzer
Specific Surface Area (m2/g) 0.20-0.40 BET Analyzer
Specific Capacity (mAh/g) [1st cycle] 153-158 0.2C, 4.2-2.7 V vs Li/Li+, Half Cell
Columbia Efficiency (%) [1st cycle] ≥85%


Note: MTI does not manufacture this product, and only sell the small quantity to research for development for new generation battery. If you need a larger quantity or have the question for IP, we will forward your inquiry to the producer.

XRD
SEM
Particle Size


Application Notes
:

  1. Please click to see Procedure for Preparing Anode & Cathode Electrode Slurry.
  2. Please keep the powder in vacuum box to avoid moisture.
  3. Please bake the powder in a vacuum oven at 120 - 150 °C before making slurry and coating to ensure max. capacity.
View full details